Dump body repair.

Dump body rot repair. Where the side wall meets the floor of the body has heavy rot damage. The body was plated with 10 Ga steel that was bent 90 Deg for strength reinforcing the side wall. The angle adds a lot of strength the the side wall making the body solid and rigid again.